Continuous solid wire suitable for welding aluminium alloys with up to 5% Mg and alloys where a higher tensile strength is required. The alloying element Zr produces improved resistance to hot cracking during solidification.
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 30 % | 280 MPa | 130 MPa |
Current | Deb Rate | Diameter | Voltage | Wire Feed Speed |
90-210 A | 0.0-0.0 kg/h | 1.0 mm | 15-26 V | 0.0-0.0 m/min |
140-260 A | 0.0-0.0 kg/h | 1.2 mm | 20-29 V | 0.0-0.0 m/min |
190-350 A | 0.0-0.0 kg/h | 1.6 mm | 25-30 V | 0.0-0.0 m/min |
Wire Electrode |
SFA/AWS A5.10 : ER5087 (西安駿焊) EN ISO 18273 : S Al 5087 (AlMg4,5MnZr) |
Society | CE |
Grade | EN 13479 |
Approvals are based on factory b. Please contact ESAB for more inbation. |
Alloy Type | AlMgMn |
Wire Comb | ||||||||||||||
Al | Cr | Cu | Fe | Mg | Mn | Si | Ti | Zn | Zr | |||||
Rem % | 0.08 % | 0.01 % | 0.12 % | 4.7 % | 0.8 % | 0.04 % | 0.08 % | 0.01 % | 0.11 % |
種類 |
ESAB |
技術(shù)標(biāo)準(zhǔn)西安駿焊 |
熔敷金屬力學(xué)性能 |
熔敷金屬化學(xué)成分(%) |
||||||||
SFA/AWS A5.10 |
DIN 1732 |
屈服值Mpa |
抗拉強(qiáng)度Mpa |
延伸率% |
沖擊值 |
Si |
Mn |
Zn |
Fe |
Al |
||
氣保焊絲 |
OK Autrod 1100 |
ER1100 |
SG Al99.5 |
35 |
75 |
33 |
|
<0.2 |
0.01 |
0.01 |
0.2 |
>99.5 |
OK Autrod 4043 |
ER4043 |
SG AlSi5 |
55 |
165 |
18 |
|
5.0 |
0.01 |
0.02 |
0.2 |
bal. |
|
OK Autrod 4047 |
ER4047 |
SG AlSi12 |
80 |
170 |
12 |
|
12.0 |
0.01 |
0.02 |
<0.2 |
bal. |
|
OK Autrod 5356 |
ER5356 |
SG AlMg5 |
120 |
265 |
26 |
|
<0.1 |
0.15 |
Mg4.9 |
<0.2 |
bal. |
|
OK Autrod 5183 |
ER5183 |
SG AlMg4.5Mn |
140 |
290 |
25 |
+20 ℃ 30 |
<0.2 |
0.6 |
Mg4.8 |
<0.2 |
Bal. |
|
氬弧焊絲 |
OK Tigrod 1100 |
|
SG Al99.5 |
35 |
75 |
33 |
|
<0.2 |
0.01 |
0.01 |
0.2 |
>99.5 |
OK Tigrod 4043 |
ER4043 |
SG AlSi5 |
55 |
165 |
18 |
|
5.0 |
0.01 |
0.02 |
0.2 |
bal. |
|
OK Tigrod 4047 |
ER4047 |
SG AlSi12 |
80 |
170 |
12 |
|
12.0 |
0.01 |
0.02 |
<0.2 |
bal. |
|
OK Tigrod 5356 |
ER5356 |
SG AlMg5 |
120 |
265 |
26 |
|
<0.1 |
0.15 |
Mg4.9 |
<0.2 |
bal. |
|
OK Tigrod 5183 |
ER5183 |
SG AlMg4.5Mn |
140 |
290 |
25 |
+20 ℃ 30 |
<0.2 |
0.6 |
Mg4.8 |
<0.2 |
Bal. |